反应 #86692

ord-e76886c1d0aa409593546785e6c5105e

反应条件

详细条件
See reaction.notes.procedure_details.

实验过程

Powdered dextrose monohydrate (1800 lbs) and powdered anhydrous citric acid (300 lbs) were combined in a 2000-gallon mixing tank that contained 743.2 gallons of soft water. To this mixture were added 52.9 gallons of 19% aqueous ammonia under agitation, and agitation was continued for approximately 30 minutes to achieve complete dissolution of solids. To the resulting solution were added 9 lbs of SILQUEST A-1101 silane to produce a pH˜8 solution (using pH paper), which solution contained approximately 25% dissolved dextrose monohydrate and dissolved ammonium citrate solids (as a percentage of total weight of solution); a 2-g sample of this solution, upon thermal curing at 400° F. for 30 minutes, would yield 15% solids (the weight loss being attributed to dehydration during thermoset binder formation). The solution was stirred for several minutes before being transferred to a binder hold tank from which it was used in the manufacture of glass fiber insulation, specifically, in the formation of a product called “air duct board.”

来源

DOI: 10.6084/m9.figshare.5104873.v1专利: US09434854B2uspto-grants-2016_09