    其他/10 min. was prepared at the rate of 0.63 kg
  2. 2
    workup.ADDITIONMonomers were mixed, pressured to 1900 kg

实验过程

A terpolymer containing 65.6 percent ethylene, 32 percent vinyl acetate, and 2.4 percent maleic anhydride, and displaying a melt index of 125 g./10 min. was prepared at the rate of 0.63 kg./hr. in a continuous 0.72-liter stirred autoclave by the following procedure. Monomers were mixed, pressured to 1900 kg./sq. cm. and fed at these rates:

来源

DOI: 10.6084/m9.figshare.5104873.v1专利: US04225476uspto-grants-1980_09