  1. 1
    workup.ADDITIONThe polymer mixture was then mixed for 30 minutes
  2. 2
    其他to provide a crosslinked polymer gel

实验过程

To the aqueous polymer mixture was added 1.0 g aluminum sulfate octadecahydrate (Sigma Aldrich, Wis.) in 50 mL deionized water. The polymer mixture was then mixed for 30 minutes to provide a crosslinked polymer gel.