反应 #155378

ord-84cac8d0701c40cc88768422185e2b4c

反应条件

详细条件
See reaction.notes.procedure_details.

实验过程

The active plug comprised: PoloXamer 188, PEO 300 000, Morphine Sulphate pentahydrate and Mannitol, which were mixed. Afterwards the powder mixture fed to the injection moulding machine.

来源

DOI: 10.6084/m9.figshare.5104873.v1专利: US08821928B2uspto-grants-2014_09