  1. 1
    Концентрированиеan aqueous solution of concentration from 1 to 10000 ppm chromium
  2. 2
    ТемператураHeat treatment at between about 100° C. and about 750° C.

Методика

In a wet chemical step, the cadmium stannate layer is treated with a solution containing chromium and/or chromium oxide, e.g. an aqueous solution of concentration from 1 to 10000 ppm chromium. Heat treatment at between about 100° C. and about 750° C. can be subsequently applied. In this way, either the cadmium stannate layer is impregnated with chromium/chromium oxide or a surface coating of chromium/chromium oxide is produced on the cadmium stannate layer.

Источник

DOI: 10.6084/m9.figshare.5104873.v1Патент: US04982135uspto-grants-1991_01