Реакция #568170

ord-c28d494043a04e55b651cb0194e12929

Уравнение реакции

CCOCCO
ethylene glycol monoethyl ether
C=Cc1ccc(OC(C)=O)cc1
4-acetoxystyrene
COCC(C)OC(C)=O
propylene glycol monomethyl ether acetate

Условия реакции

Температура
70°CELSIUS
Подробные условия
See reaction.notes.procedure_details.

Обработка

  1. 1
    ДругоеTo remove low-molecular weight oligomers and residual monomers
  2. 2
    Промывкаthis solution was washed several times with methanol/
  3. 3
    workup.ADDITIONmixed in arbitrary rate
  4. 4
    ПромывкаAfter washing

Методика

In a separable flask, 100 g of ethylene glycol monoethyl ether, 78.6 g of 4-acetoxystyrene, 21.4 g of 4-tert-butoxystyrene, and 3.7 g of dimethyl-2,2′-azobis(2-methylpropionate) as a polymerization initiator were charged and, after replacing the atmosphere in the separable flask with nitrogen, the reaction was conducted at 80° C. for 16 hours. To this reaction solution, 5 g of 25% tetramethylammonium hydroxide was added, followed by heating at 70° C. for 5 hours. To remove low-molecular weight oligomers and residual monomers, this solution was washed several times with methanol/deionized water mixed in arbitrary rate. After washing, the solvent in the solution was replaced with propylene glycol monomethyl ether acetate to obtain 400 g of a propylene glycol monomethyl ether acetate solution (solid content: 20%) of a 4-hydroxystyrene/4-tert-butoxystyrene polymer.

Источник

DOI: 10.6084/m9.figshare.5104873.v1Патент: US06653418B1uspto-grants-2003_11