Реакция #56356
ord-131f3d3a81354c29bda3691d2278ed64
Уравнение реакции
Реактанты
Реагенты
Нет
Условия реакции
Температура
500°CELSIUS
Подробные условия
See reaction.notes.procedure_details.
Обработка
- 1ДругоеThe copolymer was pumped by an extruder through a tube
- 2Другоеat 140° C
Методика
An ethylene/maleic anhydride trunk copolymer was prepared which contained 86.5 weight percent ethylene and 13.5 weight percent maleic anhydride. The copolymer was pumped by an extruder through a tube heated to about 500° C. to reduce the molecular weight. The melt viscosity was 600 centipoises at 140° C. The average chain length was about 300 carbon atoms.