Реакция #56349
ord-c6695977a3f94b0fa50fe484696ef37d
Реагенты
Нет
Условия реакции
Подробные условия
See reaction.notes.procedure_details.
Обработка
- 1Другое/10 min. was prepared at the rate of 0.63 kg
- 2workup.ADDITIONMonomers were mixed, pressured to 1900 kg
Методика
A terpolymer containing 65.6 percent ethylene, 32 percent vinyl acetate, and 2.4 percent maleic anhydride, and displaying a melt index of 125 g./10 min. was prepared at the rate of 0.63 kg./hr. in a continuous 0.72-liter stirred autoclave by the following procedure. Monomers were mixed, pressured to 1900 kg./sq. cm. and fed at these rates: