Реакция #1188
ord-daa2e4e30ef942c09a4a540a3956b1ac
Уравнение реакции
ethyl acetate
ammonium hydroxide
→
vinyl acetate
vinyl alcohol
Реагенты
Нет
Растворители
Условия реакции
Подробные условия
See reaction.notes.procedure_details.
Обработка
- 1workup.DISSOLUTIONthe polymer dissolved
- 2Другоеto give a gel
- 3ДругоеDuring the next three weeks
- 4Другоеat room temperature
- 5ТемператураAt this time the solution was heated
- 6Другоеto remove ammonia
Методика
To 100 g of the same copolymer was added 1500 ml of ethyl acetate, 40 ml of concentrated ammonium hydroxide and 40 ml of water. After two days with stirring, the polymer dissolved to give a gel. During the next three weeks at room temperature, a progressive decrease in viscosity of the solution was noted. At this time the solution was heated to remove ammonia, giving a partially saponified polymer of composition 32.4 wt % vinyl acetate, 16.4 wt % vinyl alcohol, 38 wt % TFE, and 13.2 wt % HFP in a 27.4 wt % solids solution in ethyl acetate.