  1. 1
    기타the polymer recovered
  2. 2
    workup.ADDITIONby adding the polymerization mixture to isopropyl alcohol
  3. 3
    여과The coagulated polymer was collected by filtration
  4. 4
    기타dried under reduced pressure
  5. 5
    기타Physical properties of the butadiene/styrene teleblock polymer prepared by this procedure

실험 절차

Following the completion of Step III, 2,4-di-t-butyl-4-methylphenol (one part by weight per hundred parts of total monomers) was added as a 10 weight percent solution in 50/50 (by volume) toluene/isopropyl alcohol, and the polymer recovered by adding the polymerization mixture to isopropyl alcohol. The coagulated polymer was collected by filtration and dried under reduced pressure. Physical properties of the butadiene/styrene teleblock polymer prepared by this procedure are shown in Table I.

출처

DOI: 10.6084/m9.figshare.5104873.v1특허: US04131725uspto-grants-1978_12