후처리
- 1온도heated at 130° for 2 hours
- 2기타at 150°
- 3기타2 hours
실험 절차
Resorcinol (110 g), phenyl glycidyl ether (329.5 g) and 2-phenylimidazole (0.4 ) were stirred and heated at 130° for 2 hours, then at 150° for 31/2 hours. The product had a negligible epoxy content (only 0.2 equiv./kg).