반응 #56354

ord-35eb3f27865c494eb6a02a5dc4b3fcd8

반응 방정식

C=CC(=O)OCC
ethyl acrylate
[Na+].[OH-]
sodium hydroxide
[K+].[OH-]
potassium hydroxide
C=CC(=O)OCCCC
butyl acrylate
CCOC(=O)/C=C/C(=O)[O-]
monoethyl fumarate
C=CC(=O)OCC.C=CC(=O)OCCCC.CCOC(=O)/C=C/C(=O)[O-]
Ethyl Acrylate Butyl Acrylate Monoethyl Fumarate

반응 조건

상세 조건
See reaction.notes.procedure_details.

후처리

  1. 1
    세척Coagulated polymer was washed
  2. 2
    workup.DISSOLUTIONtwice dissolved in acetone
  3. 3
    기타reprecipitated in water in a blender
  4. 4
    기타air-dried
  5. 5
    기타vacuum-oven dried 3.5 hrs
  6. 6
    기타at 72° C., and finally mill-dried at about 130° C
  7. 7
    기타The terpolymer produced

실험 절차

Coagulated polymer was washed by chopping in a blender with water, twice dissolved in acetone and reprecipitated in water in a blender, then air-dried, vacuum-oven dried 3.5 hrs. at 72° C., and finally mill-dried at about 130° C. Yield: 254 g. The terpolymer produced had an inherent viscosity (chloroform, 30° C.) of 1.51 deciliters/gram and an acid content of 0.24 meq./gram (titration with aqueous sodium hydroxide), or 0.23 meq./gram (titration with alcoholic potassium hydroxide). The terpolymer had 3.3 percent monoethyl fumarate; the remainder was believed to be about equally divided between ethyl acrylate and butyl acrylate.

출처

DOI: 10.6084/m9.figshare.5104873.v1특허: US04225476uspto-grants-1980_09