반응 #56348

ord-0efb70995f84454c851917dc994c1884

반응 방정식

C=C
ethylene
C=COC(C)=O
vinyl acetate
O=C1C=CC(=O)O1
maleic anhydride
C=C.C=COC(C)=O.O=C1C=CC(=O)O1
Ethylene/Vinyl Acetate Maleic Anhydride

반응 조건

상세 조건
See reaction.notes.procedure_details.

후처리

  1. 1
    기타/10 min. was prepared at the rate of 0.68 kg
  2. 2
    workup.ADDITIONMonomers were mixed, pressured to 1900 kg

실험 절차

A terpolymer containing 60.3 percent ethylene, 38 weight percent vinyl acetate, and 1.7 percent maleic anhydride, and displaying a melt index of 220 g./10 min. was prepared at the rate of 0.68 kg./hr. in a continuous 0.72-liter stirred autoclave by the following procedure. Monomers were mixed, pressured to 1900 kg./sq. cm., and fed at these rates:

출처

DOI: 10.6084/m9.figshare.5104873.v1특허: US04225476uspto-grants-1980_09