반응 #54212

ord-0708d5af58984a5f8a2d2c83dc6c2c80

반응 방정식

CC(C[*:1])[*:2]
polypropylene
C=C(C)C(=O)O
methacrylic acid
C=CC
propylene
C=C(C)C(=O)O
methacrylic acid

용매

반응 조건

온도
95°CELSIUS
상세 조건
See reaction.notes.procedure_details.

후처리

  1. 1
    온도The mixture was then heated at just
  2. 2
    여과The product was filtered
  3. 3
    세척washed with water
  4. 4
    기타dried in a vacuum oven at 75° C. for two hours

실험 절차

A modified resinous polymer of propylene containing approximately 10% by weight methacrylic acid was prepared as follows: 0.5 grams of Lupersol 256 Peroxide (peroxyhexanoic acid manufactured by Wallace & Tiernan Inc., Lucidol Division) was added to a reactor containing 200 grams of substantially crystalline homopolymeric polypropylene powder, 25 grams of methacrylic acid and 600 grams of water. The mixture was then heated at just below reflux temperature, about 95° C., for one hour. The product was filtered and washed with water followed by acetone and then dried in a vacuum oven at 75° C. for two hours. The modified resinous polymer of propylene weighed 225.6 grams.

출처

DOI: 10.6084/m9.figshare.5104873.v1특허: US04147741uspto-grants-1979_04