반응 #518096

ord-fa3f744e22c74ba58e4a85ae1a5fdd17

용매

반응 조건

상세 조건
See reaction.notes.procedure_details.

후처리

  1. 1
    기타precipitated resin
  2. 2
    기타the resultant was dried under reduced pressure

실험 절차

With the use of 100 g (0.567 mole) of p-tert-butoxystyrene and 5.3 g (0.03 mole) of p-tert-butylstyrene, the same polymerization reaction and after-treatment as described in Production Example 2-(1) were conducted. Then, the resulting viscous resinous material was dissolved in 300 g of acetone and poured into 2000 ml of 50% aqueous methanol solution and precipitated resin was subjected to decantation. This process step was conducted further twice, and the resultant was dried under reduced pressure to give 94.5 g of poly(p-tert-butoxystyrene/p-tert-butylstyrene) as white powders. Then, 70 g of the polymer was subjected to the same reaction and after-treatment as described in Production Example 9-(1) to give 48.5 g of poly(p-hydroxystyrene/p-tert-butylstyrene) as white powders. A ratio of p-hydroxystyrene unit and p-tert-butylstyrene unit was about 94:6 by 1HNMR. Mw: about 16000, Mw/Mn: 1.29 (GPC method: polystyrene as standard).

출처

DOI: 10.6084/m9.figshare.5104873.v1특허: US06656660B1uspto-grants-2003_12