반응 #499692

ord-247349b812b04a4781e5343d11f8e06f

반응 조건

상세 조건
See reaction.notes.procedure_details.

후처리

  1. 1
    workup.ADDITIONis introduced
  2. 2
    기타is effected at 60° C
  3. 3
    기타which is polymerized at 60° C. for 60 minutes
  4. 4
    기타recovered by steam stripping
  5. 5
    기타dried in an oven at reduced pressure at 60° C.

실험 절차

186 g of butadiene and 2.4 ml of a 0.5 M solution of tetramethylethylenediamine in cyclohexane is introduced into 4 litres of deaerated cyclohexane. After compensation for the impurities supplied by the solvent and the monomer using n-butyllithium, 3.7 ml of a 0.5 mol/l solution of n-butyllithium in cyclohexane is introduced. The polymerization of the polybutadiene block is effected at 60° C. After conversion of all the butadiene, 114 g of styrene is introduced, which is polymerized at 60° C. for 60 minutes. The copolymer is then protonated by addition of a large excess of methanol in solution in toluene, antioxidized by the addition of 2,2′- methylene bis(4-methyl-6-tert. butylphenol) (1 g per 100 g of monomer), then recovered by steam stripping and dried in an oven at reduced pressure at 60° C.

출처

DOI: 10.6084/m9.figshare.5104873.v1특허: US06562923B1uspto-grants-2003_05