  1. 1
    온도After this temperature was maintained for 4 hours
  2. 2
    온도the catalyst was cooled, in a stream of dry nitrogen, to room temperature
  3. 3
    workup.ADDITIONto mix on a roller for about 16 hours
  4. 4
    기타to evaporate at room temperature

실험 절차

An iron containing ZSM-5 catalyst was prepared by the following method: 7.6 g of the same HZSM-5 as that of Example 1 was heated in a stream of dry nitrogen to 375° C. After this temperature was maintained for 4 hours, the catalyst was cooled, in a stream of dry nitrogen, to room temperature. A solution of 0.5 g of ferrocene (dicyclopentadienyliron) in 30 g dry benzene was then added to the calcined zeolite and the slurry allowed to mix on a roller for about 16 hours. The benzene was allowed to evaporate at room temperature to give a benzene/ferrocene wetted zeolite. This wet solid was then heated to a temperature that did not exceed 100° C. in a vacuum oven so as to remove the residual benzene. This dry catalyst was then calcined in a stream of air at about 450° C. for about 6 hours to produce the desired iron containing catalyst, Catalyst A. The iron loading of this catalyst is about 1.8 wt. %.

출처

DOI: 10.6084/m9.figshare.5104873.v1특허: US05482692uspto-grants-1996_01