  1. 1
    기타One operates under the same polymerization conditions in 250 cc
  2. 2
    기타Copolymerization

실험 절차

One operates under the same polymerization conditions in 250 cc. Steinie bottles, in heptane medium (123 g.) with 9.24 g. of isoprene and 3.08 g. of styrene (25% referred to the isoprene). Copolymerization is effected for 2 hours at 70° C. in the presence of 50 × 10-6 moles of active n-BuLi.

출처