O.O.O=S(=O)([O-])[O-].[Ca+2]
land plaster
O.O.O=S(=O)([O-])[O-].[Ca+2]
calcium sulfate dihydrate
O.O=S(=O)([O-])[O-].O=S(=O)([O-])[O-].[Ca+2].[Ca+2]
calcium sulfate hemihydrate

용매

반응 조건

상세 조건
See reaction.notes.procedure_details.

실험 절차

The calcination (or dehydration) step in the manufacture of stucco is performed by heating the land plaster, and generally can be described by the following chemical equation which shows that heating calcium sulfate dihydrate yields calcium sulfate hemihydrate (stucco) and water vapor: CaSO4.2H2O+heat#CaSO4.½H2O+1 ½H2O.

출처

DOI: 10.6084/m9.figshare.5104873.v1특허: US07172403B2uspto-grants-2007_02