반응 #324350
ord-1d42cfa37cac45e2a6b9d6366a68b1b8
반응 방정식
aluminum sulfate octadecahydrate
→
Aluminum Sulfate
용매
반응 조건
상세 조건
See reaction.notes.procedure_details.
후처리
- 1workup.ADDITIONThe polymer mixture was then mixed for 30 minutes
- 2기타to provide a crosslinked polymer gel
실험 절차
To the aqueous polymer mixture was added 0.4 g aluminum sulfate octadecahydrate (Sigma Aldrich, Wis.) in 50 mL deionized water. The polymer mixture was then mixed for 30 minutes to provide a crosslinked polymer gel.