반응 #2063071
ord-43a23beb0e4e480a8b474e2599a4b5d1
반응 방정식
반응물
시약
반응 조건
후처리
- 1기타After a high molecular weight was achieved by the reaction
- 2기타the resultant product was precipitated in an ethyl ether or hexane solvent
- 3기타The gathered precipitate was dried
- 4기타was obtained at a yield of about 82%
실험 절차
Propyl maleimide (1 mol.), t-butyl 5-norbornene-2-carboxylate (0.5 mol.), and 3-hydroxypropyl 5-norbornene-2-carboxylate (0.5 mol.) were dissolved in 50 g to 300 g of tetrahydrofuran (THF), 2 g to 15 g of 2,2′-azobisisobutyronitrile (AIBN) were added thereto, then the resultant solution was reacted at a temperature of 60° C. to 70° C. in a nitrogen atmosphere for 10 hours. After a high molecular weight was achieved by the reaction, the resultant product was precipitated in an ethyl ether or hexane solvent. The gathered precipitate was dried, and the desired poly(propyl maleimide/t-butyl 5-norbornene-2-carboxylate/3-hydroxypropyl 5-norbornene-2-carboxylate) polymer was obtained at a yield of about 82%. NMR spectra of the polymer is illustrated in FIG. 3.