反応 #56349
ord-c6695977a3f94b0fa50fe484696ef37d
反応方程式
ethylene
vinyl acetate
maleic anhydride
→
Ethylene/Vinyl Acetate Maleic Anhydride
反応条件
詳細条件
See reaction.notes.procedure_details.
後処理
- 1その他/10 min. was prepared at the rate of 0.63 kg
- 2workup.ADDITIONMonomers were mixed, pressured to 1900 kg
実験手順
A terpolymer containing 65.6 percent ethylene, 32 percent vinyl acetate, and 2.4 percent maleic anhydride, and displaying a melt index of 125 g./10 min. was prepared at the rate of 0.63 kg./hr. in a continuous 0.72-liter stirred autoclave by the following procedure. Monomers were mixed, pressured to 1900 kg./sq. cm. and fed at these rates: