反応 #56348
ord-0efb70995f84454c851917dc994c1884
反応方程式
ethylene
vinyl acetate
maleic anhydride
→
Ethylene/Vinyl Acetate Maleic Anhydride
反応条件
詳細条件
See reaction.notes.procedure_details.
後処理
- 1その他/10 min. was prepared at the rate of 0.68 kg
- 2workup.ADDITIONMonomers were mixed, pressured to 1900 kg
実験手順
A terpolymer containing 60.3 percent ethylene, 38 weight percent vinyl acetate, and 1.7 percent maleic anhydride, and displaying a melt index of 220 g./10 min. was prepared at the rate of 0.68 kg./hr. in a continuous 0.72-liter stirred autoclave by the following procedure. Monomers were mixed, pressured to 1900 kg./sq. cm., and fed at these rates: