反応 #551655

ord-41730fe9ee214c4fb80466baa1fae14c

反応条件

温度
100°CELSIUS
詳細条件
See reaction.notes.procedure_details.

後処理

  1. 1
    workup.ADDITIONa monomer mix
  2. 2
    workup.ADDITIONare added to the 150° C. solvent over three hours at a constant rate
  3. 3
    その他Reaction temperature
  4. 4
    workup.ADDITIONafter the addition of an initiator chaser solution

実験手順

One hundred twenty-five parts of butyl Cellosolve is heated to 150° C. and a monomer mix consisting of 200 parts of isobutyl methacrylate, 137.5 parts of n-butyl methacrylate, 50 parts of n-butyl acrylate, 62.5 parts of acrylic acid and 50 parts of methacryloxyethyl esters of linseed oil fatty acids and an initiator solution consisting of 1.5 parts of t-butyl perbenzoate dissolved in 10 parts of butyl Cellosolve are added to the 150° C. solvent over three hours at a constant rate. Reaction temperature is held at 150±2° C. throughout the gradual additions and for 15 minutes after the addition of an initiator chaser solution consisting of 3 parts of t-butyl perbenzoate dissolved in 10 parts of butyl Cellosolve. The polymer solution is then cooled to 100° C. and diluted with 174 parts of isopropanol.

出典

DOI: 10.6084/m9.figshare.5104873.v1特許: US04547556uspto-grants-1985_10