反応 #334893
ord-c5ec0c86aed749d4b5901138bf25d1f3
反応方程式
ethylene carbonate
→
ethylene carbonate
収率 98.0%
carbon dioxide
収率 10.8%
反応条件
温度
175°CELSIUS
詳細条件
See reaction.notes.procedure_details.
後処理
- 1温度is heated
実験手順
A 10:1 mole ratio of ethylene carbonate to polyglycol P-425 is heated with stirring under a nitrogen atmosphere for 6 hours at 175° C. using 0.5 percent sodium stannate trihydrate as catalyst to give 98 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 10.8 percent carbon dioxide. The catalyst is removed as in Example 1.