反応 #1929029

ord-ac17467dce5445a2829b9db64e81d07e

反応方程式

O
water
OCCO
ethylene glycol
CCCCC(CC)CCC(CC(C)C)OS(=O)(=O)[O-].[Na+]
Tergitol
OCC(O)CO.OCCO
Ethylene Glycol Glycerol

溶媒

反応条件

詳細条件
See reaction.notes.procedure_details.

実験手順

A copper oxide dispersion was produced by mixing 2.0 g NanoArc® copper oxide, 4.9 g deionized water, 0.10 g PVP K-30, 0.5 g ethylene glycol, 0.03 g Tergitol® TMN-6, 0.01 g Dynol® 604, and 1.32 g glycerol in a 20 mL vial. 5 g of zirconium oxide milling media was added and the vial was agitated for 60 minutes.

出典

DOI: 10.6084/m9.figshare.5104873.v1特許: US08945686B2uspto-grants-2015_02