反応 #1824315
ord-f9d5baca05344ad3870c5365b78923f5
反応条件
温度
80°CELSIUS
詳細条件
See reaction.notes.procedure_details.
実験手順
The same starting materials as those of Example 1 were used. That is, the sodium aluminate solution was heated at 90° C. and was stirred, and to which was mixed the sodium silicate solution heated at 80° C. over a period of about 4 minutes so that the total amount of the reaction solution was 1.75 kg in a 2-liter stainless steel container, in order to form a wholly homogeneous gel-like sodium aluminosilicate having the following molar composition.