Mode opératoire

The procedure of D(1) above was repeated except that 0.75 gram of ethylene diacrylate was used in place of the allyl acrylate, and the amount of maleic anhydride was increased to 30 grams. Yield: 417 grams. The branched tetrapolymer had about 50 mole percent of ethylene units, the units being arranged -(E)-(B')-, as in D(2). The weight percent of maleic anhydride was 3.9.

Source

DOI: 10.6084/m9.figshare.5104873.v1Brevet: US04225476uspto-grants-1980_09