Réaction #324370

ord-31631c81520743ecb2d1a43171b221ea

Équation de réaction

CCO
ethanol
COCC(C)OC(C)=O
PGMEA
CCO[Si](OCC)(OCC)OCC
TEOS
O=[N+]([O-])O
nitric acid
CCCCO
butanol
O=C(O)c1ccc2c(c1)C(=O)OC2=O
TMAN

Réactifs

Aucun

Solvants

Conditions de réaction

Température
81°CELSIUS
Conditions détaillées
See reaction.notes.procedure_details.

Traitement

  1. 1
    workup.ADDITIONwas poured
  2. 2
    Températurethe reaction mixture was heated
  3. 3
    Températurebefore cooling down
  4. 4
    workup.STIRRINGstirred at room temperature overnight

Mode opératoire

To the solvents of 60 g ethanol and 30 g PGMEA, 33.33 g TEOS, 5.71 g VTEOS and 2.40 g PTEOS monomers were individually added. While stirring a mixture of 1.13 g 0.1N nitric acid and 18.92 g water was poured, the reaction mixture was heated to reflux at 81° C. for 4 hours before cooling down. 8.84 g butanol was added to the reaction mixture and stirred at room temperature overnight. The resulting polymer was measured to have a molecular weight of Mn=1121 amu, Mw=1723 amu analyzed using the same GPC system as mentioned above.

Source

DOI: 10.6084/m9.figshare.5104873.v1Brevet: US08642246B2uspto-grants-2014_02