Réaction #2358

ord-d7d2ca3c29b649f5856b09db139c04ce

Réactifs

Aucun

Conditions de réaction

Conditions détaillées
See reaction.notes.procedure_details.

Traitement

  1. 1
    AutreThe copolymer was dried under vacuum (0.1 mm Hg) at 80° C. for about 80 hours
  2. 2
    Autreto remove any unreacted monomer
  3. 3
    Autreat 25° C
  4. 4
    Autreat room temperature

Mode opératoire

The procedure in Example 5A was substantially repeated, except that 68.48 grams (0.60 mole) of ε-caprolactone and 40.83 grams (0.40 mole) of p-dioxanone were used. The copolymer was dried under vacuum (0.1 mm Hg) at 80° C. for about 80 hours to remove any unreacted monomer. The copolymer had an inherent viscosity of 0.19 dL/g in HFIP at 25° C. The copolymer was a liquid at room temperature. The molar ratio of PCL/PDS was found to be 57.2/42.8 by proton NMR.

Source

DOI: 10.6084/m9.figshare.5104873.v1Brevet: US05728752uspto-grants-1998_03