Réaction #1553173

ord-e013514b760d44ebb5cb9a4bd9690b5c

Solvants

Conditions de réaction

Conditions détaillées
See reaction.notes.procedure_details.

Traitement

  1. 1
    FiltrationThe resin is filtered off with suction
  2. 2
    Lavagewashed twice each with 20 ml each of DMF, THF and DCM
  3. 3
    Autredried under high vacuum

Mode opératoire

2 g of the polymeric support resin from Example 8A (loading about 1.36 mmol/g, 2.72 mmol) are suspended in 20 ml of DMF and shaken with 1.23 g (5.98 mmol) of 1-azabicyclo[2.2.2]oct-3-ylacetic acid hydrochloride and 130 mg (1.09 mmol) of DMAP for 10 min. Then 1.06 ml (6.80 mmol) of N,N′-diisopropylcarbodiimide are added, and the mixture is shaken overnight. The resin is filtered off with suction, washed twice each with 20 ml each of DMF, THF and DCM and dried under high vacuum. 2.318 g of the polymer-bound title compound are obtained.

Source