Condiciones de reacción

Temperatura
500°CELSIUS
Condiciones detalladas
See reaction.notes.procedure_details.

Tratamiento posterior

  1. 1
    OtroThe copolymer was pumped by an extruder through a tube
  2. 2
    Otroat 140° C

Procedimiento

An ethylene/maleic anhydride trunk copolymer was prepared which contained 86.5 weight percent ethylene and 13.5 weight percent maleic anhydride. The copolymer was pumped by an extruder through a tube heated to about 500° C. to reduce the molecular weight. The melt viscosity was 600 centipoises at 140° C. The average chain length was about 300 carbon atoms.

Fuente