Reacción #56349

ord-c6695977a3f94b0fa50fe484696ef37d

Ecuación de reacción

C=C
ethylene
C=COC(C)=O
vinyl acetate
O=C1C=CC(=O)O1
maleic anhydride
C=C.C=COC(C)=O.O=C1C=CC(=O)O1
Ethylene/Vinyl Acetate Maleic Anhydride

Reactivos

Ninguno

Condiciones de reacción

Condiciones detalladas
See reaction.notes.procedure_details.

Tratamiento posterior

  1. 1
    Otro/10 min. was prepared at the rate of 0.63 kg
  2. 2
    workup.ADDITIONMonomers were mixed, pressured to 1900 kg

Procedimiento

A terpolymer containing 65.6 percent ethylene, 32 percent vinyl acetate, and 2.4 percent maleic anhydride, and displaying a melt index of 125 g./10 min. was prepared at the rate of 0.63 kg./hr. in a continuous 0.72-liter stirred autoclave by the following procedure. Monomers were mixed, pressured to 1900 kg./sq. cm. and fed at these rates:

Fuente

DOI: 10.6084/m9.figshare.5104873.v1Patente: US04225476uspto-grants-1980_09