Reacción #50429
ord-8bd64f4ff23f4f9898dd95212128cc50
Ecuación de reacción
Reactantes
Reactivos
Ninguno
Condiciones de reacción
Condiciones detalladas
See reaction.notes.procedure_details.
Tratamiento posterior
- 1OtroThe same procedure as in Preparation Example 4
Procedimiento
The same procedure as in Preparation Example 4 was effected except that 6 mols of L-lactide and 14 mols of ε-caprolactone were used, thereby obtaining a lactic acid-hydroxycaproic acid copolymer (hereinafter referred to as "PCLA2"). This PCLA2 had a weight average molecular weight of 72000, and a molar ratio of a lactic acid unit to a hydroxycaproic acid unit in the copolymer was 33 to 67.