  1. 1
    workup.ADDITIONThe polymer mixture was then mixed for 30 minutes
  2. 2
    Otroto provide a crosslinked polymer gel

Procedimiento

To the aqueous polymer mixture was added 0.2 g aluminum sulfate octadecahydrate (Sigma Aldrich, Wis.) in 50 mL deionized water. The polymer mixture was then mixed for 30 minutes to provide a crosslinked polymer gel.

Fuente

DOI: 10.6084/m9.figshare.5104873.v1Patente: US08641869B2uspto-grants-2014_02