Reacción #2355

ord-e82a49eb230f455cbaf06730dd7d2f50

Reactivos

Ninguno

Disolventes

Condiciones de reacción

Condiciones detalladas
See reaction.notes.procedure_details.

Tratamiento posterior

  1. 1
    Otroat 25° C.

Procedimiento

The procedure in Example 3 was substantially repeated, except that 4.4 mL (60 mmol) propylene glycol (USP grade) was used instead of 5.6 mL of 1-dodecanol. The copolymer had an inherent viscosity of 0.17 dL/g in HFIP at 25° C.

Fuente

DOI: 10.6084/m9.figshare.5104873.v1Patente: US05728752uspto-grants-1998_03