Reacción #1188

ord-daa2e4e30ef942c09a4a540a3956b1ac

Ecuación de reacción

CCOC(C)=O
ethyl acetate
[NH4+].[OH-]
ammonium hydroxide
C=COC(C)=O
vinyl acetate
C=CO
vinyl alcohol

Disolventes

Condiciones de reacción

Condiciones detalladas
See reaction.notes.procedure_details.

Tratamiento posterior

  1. 1
    workup.DISSOLUTIONthe polymer dissolved
  2. 2
    Otroto give a gel
  3. 3
    OtroDuring the next three weeks
  4. 4
    Otroat room temperature
  5. 5
    TemperaturaAt this time the solution was heated
  6. 6
    Otroto remove ammonia

Procedimiento

To 100 g of the same copolymer was added 1500 ml of ethyl acetate, 40 ml of concentrated ammonium hydroxide and 40 ml of water. After two days with stirring, the polymer dissolved to give a gel. During the next three weeks at room temperature, a progressive decrease in viscosity of the solution was noted. At this time the solution was heated to remove ammonia, giving a partially saponified polymer of composition 32.4 wt % vinyl acetate, 16.4 wt % vinyl alcohol, 38 wt % TFE, and 13.2 wt % HFP in a 27.4 wt % solids solution in ethyl acetate.

Fuente

DOI: 10.6084/m9.figshare.5104873.v1Patente: US05723556uspto-grants-1998_03