Reaction #481598

ord-7b1a24fb48914cc0bd50e5d464ebaafa

Conditions

Detailed conditions
See reaction.notes.procedure_details.

Procedure

A zirconium-cerium-lanthanum composite oxide (Powder A5) was prepared according to the procedure of Example 1 while changing the amounts of zirconium oxychloride, cerium, and lanthanum to be used so as to form a weight ratio of 40 g of zirconium oxide, 10 g of cerium oxide, and 10 g of lanthanum oxide.

Source

DOI: 10.6084/m9.figshare.5104873.v1Patent: US06602479B2uspto-grants-2003_08