Reaction #481597

ord-e7962330c4504cd6866757f7e6cb0f05

Conditions

Detailed conditions
See reaction.notes.procedure_details.

Procedure

A zirconium-cerium-lanthanum composite oxide (Powder A2) was obtained according to the procedure of Example 1 while changing the amounts of zirconium oxychloride, cerium, and lanthanum to be used so as to form a weight ratio of 25 g of zirconium oxide, 12.5 g of cerium oxide, and 9.5 g of lanthanum oxide.

Source

DOI: 10.6084/m9.figshare.5104873.v1Patent: US06602479B2uspto-grants-2003_08