Reaction #2146739

ord-7015cf9b3913433e80581de2abcb85d2

Reaction equation

C=C(C)C(=O)OCCN(C)C
dimethylaminoethyl methacrylate
C=CC(=O)O
acrylic acid
C=C(C)C(=O)OCCN(C)C.C=CC(=O)O
dimethylaminoethyl methacrylate acrylic acid

Solvents

Conditions

Temperature
71°CELSIUS
Detailed conditions
See reaction.notes.procedure_details.

Workup

  1. 1
    OtherA relative permeability modifier useful in the present invention was prepared
  2. 2
    Othersparging with nitrogen for 30 minutes
  3. 3
    workup.ADDITIONfollowed by the addition of 0.2 mL of 2-mercaptoethanol and 1.3 g of 2,2′-azo bis(2-amidinopropane)dihydrochloride

Procedure

A relative permeability modifier useful in the present invention was prepared as follows. First, a polymer was made by mixing 45.0 g of dimethylaminoethyl methacrylate, 6.8 g acrylic acid, 372.0 g of water and sparging with nitrogen for 30 minutes. Thereafter, the pH was adjusted to approximately 5.3 with 5.7 mL of concentrated sulfuric acid, followed by the addition of 0.2 mL of 2-mercaptoethanol and 1.3 g of 2,2′-azo bis(2-amidinopropane)dihydrochloride. The resulting solution was then heated to 71° C., with stirring, and held for 18 hours to produce poly(dimethylaminoethyl methacrylate/acrylic acid).

Source

DOI: 10.6084/m9.figshare.5104873.v1Patent: US08278250B2uspto-grants-2012_10