Reaction #1256722

ord-65553c8be1584eafa7d45bda73d4bd69

Reaction equation

C=CC(=O)O
acrylic acid
C[NH+](C)C.[Cl-]
trimethylammonium chloride
CCCCc1ccc(C)c(O)c1CCCC
dibutylhydroxy toluene
Oc1ccccc1Cc1ccccc1O
bisphenol F

Solvents

Conditions

Temperature
98°CELSIUS
Detailed conditions
See reaction.notes.procedure_details.

Workup

  1. 1
    Otheras the polymerization inhibitor therein, then temperature
  2. 2
    Otherwas risen up to 60° C
  3. 3
    Otherwas risen up to 80° C
  4. 4
    OtherThe resultant reaction mixture
  5. 5
    Washwas washed with water, and toluene
  6. 6
    workup.DISTILLATIONwas distilled out

Procedure

Bisphenol F epoxy resin (Nihon Kayaku Co., Ltd. RE-404P, epoxy equivalent 160 g/eq., amount of hydrolysis 30 ppm) was dissolved in toluene, and added dibutylhydroxy toluene as the polymerization inhibitor therein, then temperature was risen up to 60° C. Thereafter, acrylic acid in 100% equivalent amount to epoxy group was added, further temperature was risen up to 80° C. Then trimethylammonium chloride as the reaction catalyst was added thereto, followed by stirring at 98° C. for about 50 hours. The resultant reaction mixture was washed with water, and toluene was distilled out to obtain epoxy acrylate of bisphenol F (Epoxyacrylate C).

Source

DOI: 10.6084/m9.figshare.5104873.v1Patent: US07824746B2uspto-grants-2010_11