Reaktion #73696
ord-17854a65b2ca4c51ba1e4ccb6763ab31
Reaktionsgleichung
Reagenzien
Keine
Lösungsmittel
Reaktionsbedingungen
Detaillierte Bedingungen
See reaction.notes.procedure_details.
Aufarbeitung
- 1workup.STIRRINGThe mixture was stirred for 23 hours at a temperature between about 210° F. and about 225° F
- 2workup.STIRRINGwith stirring
- 3workup.STIRRINGThe mixture was stirred under vacuum for 5 hours at a temperature between about 215° F. and about 235° F.
- 4Sonstigeto give a liquid soybean oil
Vorschrift
The above amounts of diethanolamine and iodine were added to the above amount of soybean oil with stirring. The mixture was stirred for 23 hours at a temperature between about 210° F. and about 225° F. Then, the above amounts of maleic anhydride, diethylene glycol, and p-toluenesulfonic acid were added with stirring. The mixture was stirred under vacuum for 5 hours at a temperature between about 215° F. and about 235° F. to give a liquid soybean oil based polyol with a hydroxyl number of 54. A reaction mixture of about 10.00 grams of the polyol and the above indicated amount of diphenylmethane diisocyanate yielded a solid soybean oil based polyurethane material.