Reaktion #429979

ord-8f1825e9c51041d3b604cf6789ec8c83

Lösungsmittel

Reaktionsbedingungen

Detaillierte Bedingungen
See reaction.notes.procedure_details.

Aufarbeitung

  1. 1
    SonstigeThe procedure used for the preparation of copolymer S-1
  2. 2
    SonstigeA tacky amorphous polymer was obtained in 65% conversion

Vorschrift

The procedure used for the preparation of copolymer S-1 was repeated except that 1-hexene was replaced with 1-decene. A tacky amorphous polymer was obtained in 65% conversion having an inherent viscosity of 4.2 dL/g in n-hexane and a Tg of -45° C. It contained 91 mole percent of 1-decene and 9 mole percent of ethylene.

Quelle

DOI: 10.6084/m9.figshare.5104873.v1Patent: US05859088uspto-grants-1999_01