Reaktion #343031

ord-fa3d8876aad740bf8c2541a50d121341

Reaktionsbedingungen

Detaillierte Bedingungen
See reaction.notes.procedure_details.

Vorschrift

The emulsion was chemically and optically sensitized, and then coated at the coverage rate of 0.5 grams per square meter with a silver to gelatin ratio of 0.3 and hydroquinone and phenidone thus obtaining a gelatin/hydroquinone/phenidone ratio of 1:0.07:0.01.

Quelle

DOI: 10.6084/m9.figshare.5104873.v1Patent: US04699868uspto-grants-1987_10