Reaktion #324349

ord-4cd56d4db15e435d9930ea75a1220027

Reaktionsgleichung

O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O=S(=O)([O-])[O-].O=S(=O)([O-])[O-].O=S(=O)([O-])[O-].[Al+3].[Al+3]
aluminum sulfate octadecahydrate
O=S(=O)([O-])[O-].O=S(=O)([O-])[O-].O=S(=O)([O-])[O-].[Al+3].[Al+3]
Aluminum Sulfate

Lösungsmittel

Reaktionsbedingungen

Detaillierte Bedingungen
See reaction.notes.procedure_details.

Aufarbeitung

  1. 1
    workup.ADDITIONThe polymer mixture was then mixed for 30 minutes
  2. 2
    Sonstigeto provide a crosslinked polymer gel

Vorschrift

To the aqueous polymer mixture was added 0.4 g aluminum sulfate octadecahydrate (Sigma Aldrich, Wis.) in 50 mL deionized water. The polymer mixture was then mixed for 30 minutes to provide a crosslinked polymer gel.

Quelle

DOI: 10.6084/m9.figshare.5104873.v1Patent: US08641869B2uspto-grants-2014_02