Reaktion #308367
ord-b80ea75d1a654cc59ecbbeb9f1e5f6b8
Reaktionsgleichung
Edukte
Reagenzien
Keine
Lösungsmittel
Reaktionsbedingungen
Detaillierte Bedingungen
See reaction.notes.procedure_details.
Vorschrift
In the absence of light, the precipitated CdSe nanocrystals are dissolved in the MUA-methanol solution. The resulting solution is stirred under an Argon flow for about 2 hours to form mercaptoundecanoic acid (MUA)-capped CdSe nanocrystals. Ethyl acetate and ethyl ether are used to precipitate and wash (repeatedly between about 2 and 3 times) the MUA-capped CdSe nanocrystals. Subsequently, the MUA-capped CdSe nanocrystals preferably are dispersed in isopropanol to define a cadmium selenide (CdSe) solution.