Reaktion #2487425

ord-8cf1d7c926d84faab3d5b2f967e81a26

Reaktionsgleichung

C=CC(=O)OC1CCCCC1.C=Cc1ccc(OC(C)(C)C)cc1
p-tert-butoxystyrene cyclohexyl acrylate
Cl
hydrochloric acid
C=CC(=O)OC1CCCCC1.C=Cc1ccc(O)cc1
p-hydroxystyrene cyclohexyl acrylate

Lösungsmittel

Reaktionsbedingungen

Temperatur
75°CELSIUS
Detaillierte Bedingungen
See reaction.notes.procedure_details.

Aufarbeitung

  1. 1
    Temperaturafter cooling
  2. 2
    Sonstigeto precipitate the reaction product
  3. 3
    FiltrationThe precipitated solid was collected by filtration
  4. 4
    Waschenwashed with water
  5. 5
    Sonstigedried under reduced pressure

Vorschrift

130.5, Gram of poly(p-tert-butoxystyrene/cyclohexyl acrylate) was suspended in isopropanol, and 30 mL of concentrated hydrochloric acid was added to the suspension. This mixture was stirred at 70 to 80° C. over 4 hours and after cooling, the reaction solution was poured in 1,500 mL of water to precipitate the reaction product. The precipitated solid was collected by filtration, washed with water and dried under reduced pressure. In this way, 85.5 g of poly(p-hydroxystyrene/cyclohexyl acrylate) was obtained as a white powder crystal.

Quelle

DOI: 10.6084/m9.figshare.5104873.v1Patent: US08795945B2uspto-grants-2014_08