Reaktion #2307225

ord-df306f933b594fc1aa54f40d4798c487

Reaktionsgleichung

C=CC(=O)OCCCCCCCCCCCCCCCCCCCCCC
behenyl acrylate
C=C(C)C(=O)OCCCCCCCCCCCC
lauryl methacrylate
C=C(C)C(=O)OCCCCCCCCCCCC.C=CC(=O)OCCCCCCCCCCCCCCCCCCCCCC.C=COC(C)=O
behenyl acrylate lauryl methacrylate vinyl acetate

Lösungsmittel

Reaktionsbedingungen

Temperatur
60°CELSIUS
Detaillierte Bedingungen
See reaction.notes.procedure_details.

Aufarbeitung

  1. 1
    Sonstigeequipped with a stirrer
  2. 2
    Sonstigea heater, a thermometer and a nitrogen-bubbling duct
  3. 3
    SonstigeThe reactor is flushed with nitrogen gas
  4. 4
    Sonstigesealed
  5. 5
    workup.ADDITIONThen vinyl acetate (2 g) is charged
  6. 6
    workup.ADDITION2,2′-azobis(2-methyl, ethyl-propionitrile) (0.06 g) is added
  7. 7
    TemperaturThe reaction mixture is heated in the closed system at 80° C. for two hours

Vorschrift

Xylene (15 g), behenyl acrylate (15 g) and lauryl methacrylate (2 g), are charged to a reactor equipped with a stirrer, a heater, a thermometer and a nitrogen-bubbling duct. The reactor is flushed with nitrogen gas and sealed. Then vinyl acetate (2 g) is charged. The reactor is heated to 60° C. and 2,2′-azobis(2-methyl, ethyl-propionitrile) (0.06 g) is added. The reaction mixture is heated in the closed system at 80° C. for two hours to provide behenyl acrylate/lauryl methacrylate/vinyl acetate polymer having a number average molecular weight of 47,750 Daltons with polydispersity 4.5. The viscosity of the polymer is 168 cP at 20° C. as a 40% solution in toluene.

Quelle

DOI: 10.6084/m9.figshare.5104873.v1Patent: US07417009B2uspto-grants-2008_08