One half of the exposure zone (5.7 cm. by 5.7 cm.) of NESA glass plate 12 was coated with a 20 micron thick layer of a dark charge exchange layer 13 composed of 2,4,7-trinitro-9-fluorenone and a Butvar binder as described in the formulation given in Example 6. The other half of the NESA glass plate 12 was left uncoated.