  1. 1
    workup.ADDITIONto mix for approximately 2 hours
  2. 2
    أخرىThe resulting solution was then spray dried

الإجراء التجريبي

An aqueous solution of malic acid was prepared by mixing 134.09 g of malic acid with 50 mL of water. An aqueous solution of calcium oxide was also prepared in a separate container by thoroughly mixing 56.08 g of calcium oxide in 50 mL of water. Next, 54.94 g of ferronyl powder was then added to the malic acid solution. The calcium oxide solution was then slowly added to the iron/malic acid solution. The solution was allowed to mix for approximately 2 hours. The resulting solution was then spray dried to produce a powdered dihydroxycalcium ferrous malate (or calciumhydroxy ferroushydroxy malate).

المصدر

DOI: 10.6084/m9.figshare.5104873.v1براءة الاختراع: US06706904B1uspto-grants-2004_03